Materials
Metal Materials for Part Fabrication
When selecting the right materials for your next sheet metal or CNC machining project, it’s important to review the physical properties and available surface finishing to ensure a good fit. See the table below for an introduction to the commonly used metal materials in our China sheet metal manufacturing facility.
Material | Surface finish | Yield (MPA) | Tensile (MPA) | Hardness | GB standard | Sheet Metal | CNC Turning | ||||
---|---|---|---|---|---|---|---|---|---|---|---|
Powder coating | E-Coating | Zinc plating | Anodized | Passivation | |||||||
Cold Rolled Steel (CRS) | |||||||||||
SPCC | ≥210 | ≥350 | HB 65 - 80 | JIS G3141-2009 | |||||||
SAPH440 | ≥305 | ≥440 | HB 80 ±30 | Q/BQB 310-2009 | |||||||
Hot Rolled Steel | |||||||||||
#20 | ≥245 | ≥410 | ≥143 | GB/20CrNiMo | |||||||
Q235 | ≥235 | 375 – 500 | HB 120 ±40 | GB/T 700-2006 | |||||||
Q345 | ≥345 | 490 – 675 | HB 120 ±40 | GB/T 1591-2008 | |||||||
Spring Steel | |||||||||||
65Mn | ≥785 | ≥980 | HB 190 – 340 | GT/T 1222-2007 | |||||||
Aluminum | |||||||||||
AL1060 | ≥35 | ≥75 | HB 26 ±5 | GB/T 3190-2008 | |||||||
AL5052 H32 | ≥70 | 210 – 260 | HV 11 ±2 | GB/T 3190-2008 | |||||||
AL6061 T6 | ≥276 | ≥260 | HV 15 – 18 | GB/T 3190-2008 | |||||||
AL6063 T5 | ≥170 | ≥250 | HB 25 ±5 | GB/T 3190-2008 | |||||||
AL7075 T6 | ≥503 | ≥572 | HB 150 ±5 | GB/T3880-2017 | |||||||
Stainless Steel | |||||||||||
SS301 | ≥205 | ≥520 | HB 76 – 187 | GB/T 8170-2008 | |||||||
SS304 | ≥205 | ≥520 | HB 76 – 187 | GB/T 24511-2009 | |||||||
SS316 | ≥205 | ≥520 | HB 76 – 187 | GB/T 24511-2009 | |||||||
Cold Galvanized Steel | |||||||||||
SGCC | ≥200 | ≥380 | HB 50 – 65 | JIS-G3302 |
Check all the information about Surface finishing Types, properties, colors and more!